The panels are manufactured to a density of 31 pet (0.50 specific gravity) to 55 pcf (0.88 specific gravity) by the application of heat and pressure by a process in which the interfiber bond is substantially created by the added binder. Other materials... A Compendium of Information on Selected Low-cost Building Materials - Page 72 edited by - 1988 - 106 pages Full view -
|